05). The lowest SBS values were observed for Vertise Flow (2.3 ± 1.47 MPa) (P ≤ .05) and were below the acceptable limit of 5 MPa. All of the investigated repair materials in combination with the ceramic veneers exhibited ΔE values that were higher than the clinically acceptable limits. Thermal aging negatively affected the SBS values in all groups (P ≤ .05). All tested self-adhesive composite resins, with the exception of Vertise Flow, could be used instead of a repair kit with flowable composite resin, especially in noncooperative