An amendment to this paper has been published and can be accessed via a link at the top of the paper.In this study, Zn/Cu-bearing smelting slag was recycled via an integrated acid dissolution and hematite precipitation method. The slag was dissolved in nitric acid to generate an acid solution containing 23.5 g/L Fe, 4.45 g/L Zn and 2.81 g/L Cu, which was subjected to hydrothermal treatment with the addition of levulinic acid (LA). More than 99.95% of the initial Fe content was removed as hematite particles with diameters of approxima