https://www.selleckchem.com/products/10074-g5.html
% of Sn was varied in the alloy and the evolution of the microstructure was described clearly. Mechanical properties of Mg-Sn alloys were improved, as the Sn content increased up to 5 wt.% and declined in the case of a 10 wt.% Sn addition. A similar trend was observed even in the case of corrosion resistance and bioactivity properties. Among the alloy compositions studied, Mg with a 5 wt.% addition has proved to be a promising candidate material for orthopedic implant applications with an acceptable elastic modulus, higher corrosion re