SEM showed the presence of a reacted layer of glass particles in the composite surface and the presence of a surface layer of apatite in AS7. The compressive strength and flexural strength were significantly higher for the silylated BG composites. The strengths of both silylated and non silylated BG composites and IG composites decreased upon immersion. BG composites exhibit reduced strengths upon immersion but still exhibit strengths comparable to existing composites after 84 days of immersion. BG composites exhibit reduced strengths