14 w - Translate

https://www.selleckchem.com/mTOR.html
Phosphoric acid-modified biochar (PMBC) was prepared using biochar (BC) as the carbon source and phosphoric acid as the activating agent. The PMBC exhibited an ordered vessel structure after deashing treatment, but the sidewalls became much rougher, the polarity (O/C atomic ratio of BC = 0.2320 and O/C atomic ratio of PMBC = 0.1604) decreased, and the isoelectric points (PI of BC = 5.22 and PI of PMBC = 5.51) and specific surface area (SSA of BC = 55.322 m2/g and SSA of PMBC = 62.285 m2/g) increased. The adsorption characterization of the removal o