The other two groups were similar to each other and the control. The composite containing particles with 88h crosslinking time showed the lowest flexural strength at 7 days in water, and materials with non-crosslinked particles and longer crosslinking time presented flexural strength similar to control. The flexural modulus and DC showed no statistical difference among groups. composite resin containing 0.5% chitosan/DCPA particles crosslinked by 16h showed a reduction of biofilm formation without affecting the mechanical properties in relation to t