51 W m-1 K-1 at 873 K is achieved in (Ca0.75Ba0.25)0.995Na0.005Mg1.95Zn0.05Bi1.98 alloy, approaching the amorphous limit. Such maintenance of high mobility and realization of ultralow lattice thermal conductivity synergistically result in broadly improvement of the quality factor β. Finally, a maximum ZT of 1.25 at 873 K and the corresponding ZT ave up to 0.85 from 300 K to 873 K have been obtained for the same composition, meanwhile possessing temperature independent compatibility factor. To our knowledge, the current ZT ave exceeds